Title: Critical helium fluence for hydrogen retention in stainless steel
Abstract: Hydrogen depth profiles have been measured for stainless steel pre-implanted with 10 keV helium ions to fluences below and above the critical fluence. We observed double peaking in the profile for a fluence of 3.2 × 1017 He cm−2, which is above the critical fluence. The double peaking was possibly caused by the onset of blistering.